As 2017 is coming to a close, it is the perfect opportunity to reflect on the exciting innovative products released over the last 12 months. These one and two part epoxy systems offer exceptional mechanical strength, superior electrical and thermal properties. They also meet strict industry standards. Without further ado, let’s take a closer look at some of the standout products of the year.
|
|
EP3HTND-2Med Black: Biocompatible Epoxy Paste Will Not Flow While Curing |
The one part epoxy meets USP Class VI specifications as well as ISO 10993-5 for cytotoxicity. EP3HTND-2Med Black possesses superior chemical resistance, particularly to chemical sterilants, as well as to other types of sterilization including EtO, radiation and especially autoclaving.
For more information, request a technical data sheet on EP3HTND-2Med Black
|
| EP3HTSCN: One Part, Electrically Conductive Epoxy |
Featuring a silver coated nickel filler, EP3HTSCN delivers low volume resistivity and affordability. This smooth paste system can still be readily dispensed from a syringe and has excellent bonding properties.
For more information, request a technical data sheet on EP3HTSCN
|
| Supreme 3HTND-2DM: Epoxy for Specialty Dam-and-Fill Encapsulation |
Supreme 3HTND-2DM is a rapid curing, toughened, one part epoxy system that passes ASTM E595 specifications for NASA low outgassing allowing it to be used in vacuum, aerospace, electro-optic and other related applications.
For more information, request a technical data sheet on Supreme 3HTND-2DM
|
|
EP93FRHT: Meets Airbus Standards for Flame Retardancy, Smoke and Toxic Gas
|
EP93FRHT is a non-halogenated system that can be used in interior panels, floor and door assemblies, as well as frame lining for a variety of aircraft.
For more information, request a technical data sheet on EP93FRHT
|
|
EP62-1BF: Low Viscosity Epoxy with Exceptional Chemical Resistance
|
EP62-1BF is a low exotherm system that has a mixed viscosity of 2,000-5,000 cps, enabling it to be used for potting small components. It is thermally stable and has a glass transition temperature (Tg) of 125-135°C.
For more information, request a technical data sheet on EP62-1BF
|
|
EP29LPHE: Very Low Viscosity Epoxy Offers Superior Impact Resistance
|
Optically clear EP29LPHE is a two component epoxy that has notable toughness along with high elongation, which imparts good impact and shock resistance. It has exceptionally low shrinkage upon cure and is ideal for larger potting applications.