This 32-page catalog offers performance properties on Master Bond’s extensive line of epoxy, silicone, polyurethane, silicate based and light curing compounds. These products provide solutions to PCB assembly, die-attach, conformal coating, surface mount, lid sealing, chip and wire bonding applications.
Download Now
image

Popular Electronic Adhesive Systems

image

Room Temperature Curing, Silver Conductive Epoxy

Silver filled, electrically conductive EP21TDCS has a convenient one to one mix ratio, by weight or volume. This two part adhesive readily develops high strength bonds after curing that are resistant to thermal cycling and many chemicals. It is serviceable over the wide temperature range of 4K to +275°F enabling it to be used in cryogenic applications.
For more information, request a technical data sheet on EP21TDCS
image

Thermally Conductive, Electrically Insulative System

EP30AO has an attractive balance of high physical strength and dimensional stability for a variety of electronic applications. In particular, its low viscosity and superior flow properties make it an ideal potting compound. This system forms rigid bonds that are resistant to water and many chemicals including oil and most solvents.
For more information, request a technical data sheet on EP30AO
image

Silicone System for Electro-Optical Components

Featuring unsurpassed thermal stability, MasterSil 800 is serviceable at temperatures as high as 300°C. This one part, high performance, non-corrosive silicone is low in viscosity making it free flowing and self leveling. It is ideal for bonding, sealing, protective coatings, encapsulating and creating formed-in-place gaskets.
For more information, request a technical data sheet on MasterSil 800
image

Soft & Resilient Sealing & Encapsulation Compound

Super Gel 9 is a urethane modified epoxy that features unmatched performance properties including dimensional stability, easy repairability and can be cast up to 2-3 inches thick. Its combination of properties enables it to be used for encapsulating sensitive electronic parts and sealing delicate optical components.
For more information, request a technical data sheet on Super Gel 9
image

Exceptionally High Glass Transition Temperature

UV10TK40 features temperature resistance up to 450°F and a glass transition temperature of 140°C. This one part, high viscosity UV system also offers excellent dimensional stability. Optically clear UV10TK40 can cure in sections up to 0.090-0.100 inches when exposed to a UV light source.
For more information, request a technical data sheet on UV10TK40
image

Toughened, Thermally Conductive Epoxy

Supreme 10AOHT withstands rigorous thermal cycling over the wide service temperature range of 4K to +400°F. This one part system also offers excellent thermal conductivity and electrical insulation properties. It is widely used in electronic, electro-optic, aerospace and specialty applications where high strength, the convenience of a no mix system, excellent thermal transfer properties and high temperature resistance are required.
For more information, request a technical data sheet on Supreme 10AOHT