Featuring an extraordinary combination of properties, EP3SP5FL is a one component epoxy offering snap cures of 1-2 minutes at 300°F. It has high strength properties, superior electrically insulation and is readily reworkable. Additionally, it can withstand exposure to thermal cycling.

Read More
“3 Minute" Cure Epoxy
image
Master Bond EP51M epoxy system is fast curing making it ideal for high speed production line assembly bonding operations. It produces durable and strong bonds that are resistant to thermal cycling and a variety of chemicals. Serviceable from 4K to 250°F, EP51M bonds well to dissimilar substrates. With a convenient one to one mix ratio, it is also easy to use.

For more information, request a technical data sheet on EP51M
Optically Clear Adhesive, Sealant and Coating
image
Single component UV15-7 delivers superior physical strength properties, low shrinkage upon curing and good non-yellowing stability. This system bonds well to a wide variety of substrates including glass, metals and plastics, such as polycarbonates, acrylics and a number of polyester films. It exhibits an exceptional combination of properties including outstanding durability, and good electrical insulation properties, along with noteworthy thermal cycling capabilities.

For more information, request a technical data sheet on UV15-7
Complies with MIL-A-46146A Type 1
image
Well suited for the aerospace and electronic industries, MasterSil 710 is a one part silicone system for bonding, sealing, coating and formed in place gasket applications. This non-corrosive, fast setting system has a paste consistency and cures readily at room temperature depending on the thickness of the layer and the humidity. It is translucent and is serviceable over the wide temperature range of -75°F to +400°F.

For more information, request a technical data sheet on MasterSil 710
Rapid Setting Silver Conductive Epoxy Adhesive
image
Master Bond EP77M-F delivers a very low volume resistivity of <0.001 ohm-cm. Unlike the majority of two part, silver conductive epoxy systems, EP77M-F has a convenient, one to one mix ratio, by weight or volume. This smooth paste will set up at ambient temperatures within 5-7 minutes even when mixed in very small amounts. Full cures usually take about 8-12 hours at room temperature.

For more information, request a technical data sheet on EP77M-F
Urethane Modified Epoxy Gel is Thermally Conductive
image
Featuring exceptional softness and dimensional stability, Super Gel 9AO is a two component system that delivers superior thermal conductivity and electrical insulation values. Excellent flow properties and low exotherm enable it to be cast in larger sections up to 2-3 inches thick. Super Gel 9 combines easy handling and curing properties, making it ideal for use in a variety of applications.

For more information, request a technical data sheet on Super Gel 9AO

Master Bond

Website:www.masterbond.com
Email:[email protected]
Phone:+1 201 343 8983
Facebook   Twitter   Google Plus   Linkedin
Copyright © 2014 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.