EP21TPND: Exceptional Resistance to Fuels and Oils |
Unlike many chemical resistant materials, EP21TPND has excellent toughness and flexibility enabling it to resist rigorous thermal cycling as well as mechanical and thermal shocks. It can withstand exposure to a number of chemicals including water, gasoline, fuels, oils, hydrocarbons, hydraulic fluids, acids and bases. This epoxy polysulfide has a non-drip consistency and is widely used in the aerospace, OEM, electronic, electrical, chemical and related industries.
For more information, request a technical data sheet on EP21TPND
|
| EP21TPFL-1AO: High Thermal Conductivity & Excellent Electrical Insulation |
Master Bond EP21TPFL-1AO is an electrically insulative, two part epoxy polysulfide system with a thermal conductivity of 9-10 BTU•in/ft2•hr•°F [1.30-1.44 W/(m•K)]. As a polysulfide based system, it has very good chemical resistance, particularly to fuels, oils, hydraulic fluids and related compounds. With an elongation of 150-200%, EP21TPFL-1AO offers a high degree of flexibility and it can withstand intense thermal cycling and mechanical shock. Its low viscosity makes it well suited for potting/encapsulation.
For more information, request a technical data sheet on EP21TPFL-1AO
|
|
EP21TPFL-1: Durable System Features Low Viscosity |
Two component EP21TPFL-1 is a highly flexible epoxy/polysulfide elastomer compound for high performance bonding, sealing and casting. It is formulated to cure at room temperature or more quickly at elevated temperatures. Mixed viscosity is 2,000-4,000 cps. This compound offers outstanding resistance to fuels, water and many aggressive chemicals. It exhibits excellent bond strength to both similar and dissimilar substrates. EP21TPFL-1 has long-term durability and resistance to thermal and mechanical shock. It maintains its properties even upon prolonged exposure to adverse environmental conditions.
For more information, request a technical data sheet on EP21TPFL-1
|
| EP21TP-2: Thermal Cycling Resistance & Quick Cures |
With a convenient one to one mix ratio by weight or volume, Master Bond EP21TP-2 features superior thermal shock and chemical resistance while maintaining durable bonds to similar and dissimilar substrates. EP21TP-2 cures at ambient temperatures or more rapidly at elevated temperatures and can be applied without sagging. This tough compound is noted for its ability to withstand prolonged exposure to fuel and oils. Shore D hardness is 60-65.
For more information, request a technical data sheet on EP21TP-2
|
|
|
|
Copyright 2015 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.
|
|