September 2018
EP112LS is optically clear, features reliable non-yellowing properties and has a refractive index of 1.55. This two part epoxy is formulated for impregnation, potting, encapsulation, sealing and coating applications. View this infographic to learn more.

Read More
Some additional key properties include:

Wide service temperature range

-60°F to +450°F

Exceptionally long working life

After mixing: 2-3 days

Excellent strength profile

Tensile strength: >11,000 psi

Reliable electrical insulation

Volume resistivity: >1014 ohm-cm