Well suited for structural bonding applications, EP13LTE offers excellent adhesion to dissimilar substrates and has a stellar physical strength profile. This NASA low outgassing approved system is easy to use, doesn’t require mixing, and has an unlimited working life at room temperature. It also features high temperature resistance, dimensional stability and is able to withstand 1,000 hours at 85°C/85% RH.
|
|
Some key properties include:
|
Low thermal expansion coefficient:
15-20 x 10-6 in/in/°C
|
|
Exceptional compressive strength:
24,000-26,000 psi |
|
|
|
|
|
|
|
|
|
|