Serviceable up to +500°F, EP13SPND-2 is a one part epoxy paste for structural bonding applications. This electrically insulative system has a non-drip application feature that delivers high tensile, tensile lap shear and compressive strength of over 8,000 psi, 3,000 psi and 18,000 psi, respectively. It also offers superb dimensional stability and chemical resistance.
|
|
EP30HT
|
Featuring high light transmission properties, EP30HT resists temperatures up to 400°F. It exhibits impressive physical strength and excellent adhesion to both similar and dissimilar substrates. EP30HT has exceptionally low shrinkage after cure and forms bonds that are rigid and resistant to chemicals. This compound has a four to one mix ratio by weight and is available in convenient syringe and gun applicators.
For more information, request a data sheet on EP30HT |
|
EP21TDC-4 |
Highly flexible EP21TDC-4 is a two part epoxy for bonding, sealing and coating applications. It has a high peel strength of 30 pli and an elongation of over 200%. This system can be cured at ambient temperatures or more rapidly at elevated temperatures and bonds well to both similar and dissimilar substrates. It is recommended for adhesion to natural rubber compounds without time consuming surface preparation procedures. EP21TDC-4 can even be cured under water. Bonds have excellent resistance to vibration, impact and shock. It has superior resistance to fuels, water, oils and many chemicals.
For more information, request a data sheet on EP21TDC-4 |
| Supreme 10ANHT-LO |
Offering high strength properties, Supreme 10ANHT-LO is a single component heat curing system that is serviceable over the wide temperature range of 4K to +400°F. This toughened formulation is thermally conductive and electrically insulative. It is also dimensionally stable and withstands rigorous thermal cycling. This epoxy passes NASA low outgassing ASTM E595 testing.
For more information, request a data sheet on Supreme 10ANHT-LO |
| EP15 |
With a tensile strength in excess of 12,000 psi, EP15 is a heat curing epoxy that is utilized in testing the adhesion or cohesive strength of flame sprayed coatings, as per ASTM specification C 633. This one component epoxy is easy to handle and requires no mixing. It has a high bond strength to ceramic and metallic substrates. The cured epoxy is rigid, dimensionally stable with a service temperature range of -60°F to +250°F.
For more information, request a data sheet on EP15 |
| EP31ND |
Two component EP31ND is a room temperature curing epoxy with a paste consistency for high performance structural bonding applications featuring lap shear strengths of 4,000-4,200 psi and peel strength exceeding 50 pli. The service temperature range of EP31ND is -60 to +250°F. It combines low shrinkage upon cure along with excellent resistance to many chemicals including oil and fuels. EP31ND has excellent adhesion to a wide variety of substrates. The cured adhesive is a superb electrical insulator..
For more information, request a data sheet on EP31ND |