EP21TDCN-LO is a nickel conductive epoxy adhesive/coating for grounding, shielding and static dissipation applications. This smooth paste formulation is toughened and formulated to withstand relatively rigorous thermal cycling as well as mechanical vibration and shock. Check out this infographic to learn more.

Read More
Some additional key properties include:

NASA low outgassing

Passes ASTM E595 testing

Low volume resistivity

5-10 ohm-cm

Excellent thermal conductivity

11 BTU•in/ft2•hr•°F [1.59 W/(m•K)]

Reliable strength profile

Tensile strength: 3,000-4,000 psi