Formulated with unique optical properties, EP30-2LB blocks UV light from 200-400 nm and allows the transmission of visible light from 450-900 nm. Beyond its optical properties, EP30-2LB is a reliable structural adhesive. It is dimensionally stable and exhibits low shrinkage upon cure. This low viscosity epoxy flows smoothly and evenly, enabling it to be used for coating, bonding and sealing applications.
|
|
This optically clear, two part system passes NASA low outgassing specifications. EP30-2LB resists chemicals including water, oils, fuels, acids, bases and many solvents. Some additional properties include:
|
Superb optical clarity
Refractive index: 1.55
|
|
Wide service temperature range
-80°F to +300°F [-62°C to +149°C] |
|
High strength profile
Tensile lap shear strength: 3,000-3,200 psi
|
|
Capable electrical insulator
Volume resistivity: >1015 ohm-cm |
|
|
|
|
| EP21LSCL-1: Polymer System Features Outstanding Non-Yellowing Properties |
EP21LSCL-1 is a two component, low viscosity epoxy system featuring superb optical clarity and non-yellowing properties. This versatile system can be used for high performance coating, bonding, sealing, encapsulation and casting. EP21LSCL-1 has an exceptionally long open time and features very low exotherm, making it ideal for use in deep cross section thicknesses. It is serviceable from -60°F to +250°F and retains outstanding electrical insulation characteristics after long-term aging.
For more information, request a technical data sheet on EP21LSCL-1
|
| EP30LTE-LO: NASA Low Outgassing Certified Two Component Epoxy |
Thermally conductive and electrically insulative, EP30LTE-LO can be used in bonding, coating, sealing and encapsulation applications. Additionally, it has a remarkably low coefficient of thermal expansion of 15-18 x 10-6 in/in/°C. NASA low outgassing approved, EP30LTE-LO is also noteworthy for its high bond strength, superior dimensional stability and good flow properties. This product also withstands 1,000 hours at 85°C/85% RH.
For more information, request a technical data sheet on EP30LTE-LO
|
| UV15X-2: Optically Clear UV Curable System |
UV15X-2 is a low viscosity, UV curable adhesive, sealant, coating and encapsulation system that offers exceptional light transmission and non-yellowing properties. It has a refractive index of 1.51. This high strength compound features impressive abrasion resistance and cures in sections up to ¼ inch thick.
For more information, request a technical data sheet on UV15X-2
|
|
|
|