Master Bond EP62-1 is primarily used as an adhesive, sealant or coating. It has the ability to withstand harsh environmental conditions including exposure to acids, bases and solvents. This two part epoxy features thermal stability with a glass transition temperature exceeding 160-165°C.

Read More
Dimensionally stable, this two part epoxy has excellent physical strength properties. It has a long pot life and versatile cure schedules at moderately elevated temperatures. This system also exhibits excellent electrical insulation characteristics. Some additional properties include:

Tensile lap shear strength

2,000-2,200 psi

High elongation

3-5%

Volume resistivity

>1014 ohm-cm

Service temperature range

-60°F to +450°F [-51°C to +232°C]
For more information, request at technical data sheet on EP62-1

Master Bond

Website:www.masterbond.com
Email:[email protected]
Phone:+1 201 343 8983
Facebook   Twitter   Google Plus   Linkedin
Copyright © 2017 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.