View this email online
Logo
July 2018
MasterSil 973S-LO is a two component, silver filled silicone with superb electrical and thermal conductivity. Its exceptionally low volume resistivity of 0.004 ohm-cm allows it to be used for many different applications involving bonding, sealing and coating. It is a paste like system with minimal flow and can be utilized as a form-in-place conductive gasketing material. Service operating temperature is -120°F to +400°F [-84°C to +204°C]. MasterSil 973S-LO is vacuum compatible.

Read More
Some additional key properties include:

NASA low outgassing

Passes ASTM E595 tests

Highly flexible

Elongation: 50-100%

Addition cured silicone

Mix ratio of 100:5 by weight

Thermally conductive

9-11 BTU•in/ft²•hr•°F [1.30-1.59 W/(m•K)]
For more information, request at technical data sheet on MasterSil 973S-LO

Master Bond

Website:www.masterbond.com
Email:[email protected]
Phone:+1 201 343 8983
Facebook   Twitter   Google Plus   Linkedin
Copyright © 2018 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.