Master Bond Supreme 10HTS is a user friendly, one component, silver conductive epoxy system featuring a low volume resistivity of <0.0001 ohm-cm. It is formulated to withstand rigorous thermal cycling as well as thermal and mechanical shocks. Supreme 10HTS fully meets NASA low outgassing specifications.

Read More
MB600S
image
Master Bond MB600S is an aqueous based sodium silicate coating formulated for applications where electromagnetic interference/radio frequency interference (EMI/RFI) shielding is required. Tested according to IEEE 299, 2006 methods, MB600S was as effective as the aluminum reference with a shielding effectiveness of 95-105 dB, from 100 MHz to 2 GHz. It is easy to brush on and being water based, the system is relatively non-toxic.

For more information, request a technical data sheet on MB600S
EP21TDCS
image
Silver filled, electrically conductive, room temperature curing EP21TDCS has a convenient one to one mix ratio, by weight or volume. This two part adhesive readily develops high peel and shear strength properties and is resistant to thermal cycling and many chemicals. It is serviceable over the wide temperature range of 4K to +275°F enabling it to be used in cryogenic applications.

For more information, request a technical data sheet on EP21TDCS
EP21TDCNFL
image
With a convenient one to one mix ratio, EP21TDCNFL is a highly flexible, two part, nickel filled, electrically conductive system for high performance bonding and sealing. It readily develops a tensile lap strength more than 1,500 psi and a T-peel strength greater than 30 pli. EP21TDCNFL has a wide temperature range of 4K to +250°F. It is 100% reactive and contains not solvents or diluents.

For more information, request a technical data sheet on EP21TDCNFL
MasterSil 705C
image
Primarily selected for applications involving static dissipation or EMI/RFI shielding, MasterSil 705C has striking electrical conductivity and is used in applications where a non-metallic system is required. This carbon filled, one component product is non-corrosive and retains typical silicone type flexibility and high temperature resistance.

For more information, request a technical data sheet on MasterSil 705C
EP79
image
Electrically conductive EP79 provides cost effectiveness with its silver coated nickel filler but still exhibits low volume resistivity. This compound offers high peel strength and superior toughness. Suitable for cryogenic conditions, it has a service temperature range of 4K to +275°F. This compound also has superior thermal conductivity.

For more information, request a technical data sheet on EP79
Inside Our Lab
image
Master Bond has developed a comprehensive line of electrically conductive adhesives which have many advantages over solder or mechanical fasteners. Depending on the application requirements, Master Bond can formulate rigid as well as flexible electrically conductive systems, which offer very low volume resistivity (<0.001 ohm-cm) combined with superior temperature resistance properties. These one and two component systems feature the following fillers:
  • Graphite
  • Nickel
  • Silver coated nickel
  • Silver
Learn more about the benefits of Master Bond epoxies with excellent electrical conductivity.

Master Bond

Website:www.masterbond.com
Email:[email protected]
Phone:+1 201 343 8983
Facebook   Twitter   Google Plus   Linkedin
Copyright © 2014 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.