View this email online
Logo
May 2016
Supreme 45HTQ-4 is a toughened, silicon carbide filled epoxy with outstanding thermal stability and physical properties demonstrated in this video. Supreme 45HTQ-4 is very special in that it combines exceptional chemical, temperature and abrasion resistance. This easy handling, two part compound also features low shrinkage upon curing excellent compressive strength and high dimensional stability. It can be used for a variety of bonding, sealing, coating and casting applications in oil and chemical processing, aerospace and specialty OEM industries.

Read More
Additional properties include:

High tensile strength

8,000-9,000 psi at 75°F

Impressive compressive strength

24,000-26,000 psi at 75°F

Exceptional high/low temperature resistance

Serviceable from -100°F to +450°F

Long working life

12-24 hours at room temperature for a 100 gram batch
For more information, request at technical data sheet on Supreme 45HTQ-4
UV11-3: UV/EB Curable Coating System for Plastics
image
With superb abrasion resistance, UV11-3 is an extra-hard UV curable coating for plastic substrates. This optically clear, 100% reactive system has a low viscosity that cures readily when exposed to a UV light source or EB radiation. It exhibits excellent adhesion to polycarbonates, polymethylmethacrylates, polyvinylchlorides and other plastic substrates. UV11-3 also has high resistance to staining and many common chemicals.

For more information, request a technical data sheet on UV11-3
EP21SC-1: Outstanding Resistance to Abrasion and Chemicals
image
Featuring an array of high performance properties, Master Bond EP21SC-1 is ideal for chemical and mechanical processing applications as well as tank and chute maintenance. This exceptionally rigid material has a hardness exceeding 95 Shore D and offers impressive dimensional stability. EP21SC-1 includes a silicon carbide filler which enhances its abrasion resistance. It also withstands a wide variety of chemicals including water, acids, bases, hydraulic fluids and oils. This two component epoxy system has a one to one mix ratio by weight or volume and has a smooth paste consistency.

For more information, request a technical data sheet on EP21SC-1
EP30D-7: Moderate Viscosity Urethane-Modified Epoxy Features Outstanding Toughness
image
Versatile, two component EP30D-7 is a flexibilized, system featuring outstanding strength, abrasion resistance and superior electrical insulation characteristics. EP30D-7 does not contain any solvents, cures at room temperature, flows smoothly and is resistant to thermal cycling. It also has excellent chemical resistant properties and bonds well to metals, glass, ceramics, composites, rubbers and plastics.

For more information, request a technical data sheet on EP30D-7

Master Bond

Website:www.masterbond.com
Email:[email protected]
Phone:+1 201 343 8983
Facebook   Twitter   Google Plus   Linkedin
Copyright © 2016 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.