Supreme 62-1 has excellent physical strength properties and a glass transition temperature of 155-160°C. This two part epoxy delivers superior chemical resistance against acids, bases, many solvents and other chemicals, even at high temperatures. It has a long pot life of more than 12 hours for a 100 gram batch and versatile cure schedules at moderately elevated temperatures. It also exhibits excellent electrical insulation characteristics. Most importantly, Supreme 62-1 is a toughened system with an enhanced ability to withstand rigorous thermal cycling.

Read More
Some additional key properties include:

Superior strength profile

Tensile lap shear: 2,000-2,200 psi

Excellent toughness

Elongation: 5-10%

Wide service temperature range

-60°F to +450°F [-51°C to +232°C]

Reliable electrical insulation

Volume resistivity: >1014 ohm-cm
For more information, request at technical data sheet on Supreme 62-1

Master Bond

Website:www.masterbond.com
Email:[email protected]
Phone:+1 201 343 8983
Facebook   Twitter   Google Plus   Linkedin
Copyright © 2018 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.