Master Bond UV15DC80Med is a special dual cure epoxy based system that offers a primary cure using UV light along with a secondary heat curing mechanism. This adhesive allows for curing areas on parts that do not allow UV light curing because of “shadowing” issues. The heat curing portion of this system can be initiated at the relatively lower temperature of 80°C. It also meets USP Class VI specifications and passes ISO 10993-5 cytotoxicity testing. UV15DC80Med has very good temperature resistance along with the capability of withstanding many chemicals including liquid sterilants, radiation and even steam (autoclaving).
|
|
MasterSil 912Med
|
MasterSil 912Med is a single component silicone with a paste viscosity for bonding, sealing and coating medical devices. This non-corrosive, neutral cure compound complies with USP Class VI and ISO 10993-5 specifications. It resists many kinds of sterilization including gamma radiation, EtO and some types of liquid sterilants. The service temperature range extends from -75°F to +400°F. MasterSil 912Med withstands rigorous thermal cycling as well as thermal and mechanical shock.
For more information, request a data sheet on MasterSil 912Med |
|
LED403Med |
One part LED403Med cures in thin sections in 15-30 seconds upon exposure to a 405 nm wavelength LED light. Featuring excellent optical clarity and superior light transmission properties, it fully cures tack-free without any oxygen inhibition. This dimensionally stable system resists various sterilization methods including gamma radiation, and passes the plastics test for USP Class VI biocompatibility and ISO 10993-5 cytotoxicity requirements.
For more information, request a data sheet on LED403Med |
| EP46HT-2Med |
Master Bond EP46HT-2Med is a two component biocompatible epoxy for high performance structural bonding and casting. It is suitable for applications where resistance to temperatures from -100°F to +550°F is required and high mechanical strength/chemical resistance is needed. EP46HT-2Med is also resistant to radiation, chemical sterilants and repeated autoclaving. This compound has good flow properties, a long working life at room temperature and low exotherm upon cure.
For more information, request a data sheet on EP46HT-2Med |
| EP41SMed |
USP Class VI approved, EP41SMed is well suited for a variety of uses in disposable/reusable medical devices as an adhesive, sealant and coating. This epoxy system is very fast curing at room temperature and produces high strength rigid bonds, which are remarkably resistant to chemicals as well as cold sterilants. It has a service temperature range of -60°F to + 250°F and exceptionally low linear shrinkage upon cure. EP41SMed is easy to apply, is 100% reactive and possesses excellent electrical insulation characteristics.
For more information, request a data sheet on EP41SMed |