Featuring a unique dual cure mechanism, UV15DC80Med offers a primary cure using UV light along with a secondary heat cure that can be initiated at the low temperature of 80°C. This system was formulated for medical device assembly applications. It meets USP Class VI specifications and passes ISO 10993-5 cytotoxicity testing. UV15DC80Med has very good temperature resistance along with the ability to withstand sterilization exposure including liquid sterilants, radiation and even autoclaving. It requires no mixing, is solvent free and exhibits excellent physical strength properties.
|
Some additional properties include: |
Impressive physical strength
Tensile strength: >5,000 psi
|
|
Electrically insulative
Volume resistivity: >1014 ohm-cm |
|
Outstanding thermal stability
Glass transition temperature
with post cure: >125°C
|
|
Superior optical clarity
Refractive index, 75°F: 1.52 |
|
|
|
|
| EP62-1LPSPMed: Cryogenically Serviceable System for Bonding, Sealing, Coating, Encapsulating and Impregnation |
When a two part epoxy is ideal, Master Bond offers EP62-1LPSPMed with a convenient mix ratio of 100 to 25 by weight. This ultra low viscosity system passes biocompatibility testing. Upon mixing, the viscosity is markedly low and the working life is impressively long, 12-24 hours at room temperature. It features superior resistance to EtO, radiation, chemical sterilization and autoclaving. It can be used for both reusable and disposable medical devices. In very thin sections, this system will transmit light, but in thicker ones, it is opaque.
For more information, request a technical data sheet on EP62-1LPSPMed
|
| EP3HTND-2Med Black: Biocompatible Epoxy Paste Will Not Flow While Curing |
For medical applications where a UV system is not an option, EP3HTND-2Med Black is a one part system that combines easy processing with excellent bonding properties. It cures in 20-30 minutes at 250°F or 5-10 minutes at 300°F and adheres well to a wide variety of substrates including glass, metals, ceramics and most plastics. This paste compound meets USP Class VI specifications as well as ISO 10993-5 for cytotoxicity. EP3HTND-2Med Black possesses superior chemical resistance, particularly to chemical sterilants, as well as to other types of sterilization including EtO, radiation and especially autoclaving. The service temperature range for this product is -60°F to +400°F.
For more information, request a technical data sheet on EP3HTND-2Med Black
|
|
|
|
Copyright 2018 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.
|
|