EP62-1LPSP: Cryogenically Serviceable, High Strength Epoxy
Low viscosity, EP62-1LPSP is a two component, heat curing epoxy that features an exceptionally long working life of 12-24 hours at ambient temperatures. Its thin consistency, long open time and low exotherm allows this system to be used for moderate and larger sized electrical encapsulations. This optically clear system has outstanding thermal stability with a service temperature range extending from 4K to +400°F. EP62-1LPSP cures in 60-90 minutes at 80-100°C or 30-60 minutes at 125°C.

Read More
UV10TKLO-2: High Viscosity UV Compound Withstands Harsh Chemicals
image
UV10TKLO-2 is a special one component UV curable epoxy modified system for high performance bonding, sealing and encapsulation. This system can be cured up to 1/16 of an inch and can be easily “layered” to higher levels. Most significantly, its low outgassing properties enable this UV product to be used in a wide array of optical, electro-optical and vacuum applications that until now have been “off limits” for UV curable epoxies.

For more information, request a technical data sheet on UV10TKLO-2
Supreme 10HTS: Silver Conductive Epoxy Adhesive
image
Supreme 10HTS features a combination of high performance properties including high shear peel strength, low volume resistivity, and exceptionally easy processing. This one part system is ideal for applications that turn up the heat since it resists temperatures over 400°F. As a toughened system, it offers superior resistance to impact, thermal shock, vibration and stress fatigue cracking.

For more information, request a technical data sheet on Supreme 10HTS
EP21TCHT-1: Thermally Conductive, Electrically Insulative
image
Master Bond EP21TCHT-1 is a heat resistant, two component thixotropic paste formulated for high performance bonding and sealing applications. It features high thermal conductivity and superior electrical insulation properties with an operating temperature range of 4K to +400°F. EP21TCHT-1 is NASA low outgassing certified and is therefore highly recommended for use in vacuum environments.

For more information, request a technical data sheet on EP21TCHT-1
MasterSil 972TC-LO: Low Outgassing Silicone System
image
MasterSil 972TC-LO is capable of transferring heat while retaining superior dielectric properties. It bonds well to a wide variety of substrates, including metals, composites, glass, ceramics as well as many types of rubbers and plastics. This system has very good flexibility and high elongation. It can withstand aggressive thermal cycling as well as thermal and mechanical shock. MasterSil 972TC-LO is 100% solid and has a white color.

For more information, request a technical data sheet on MasterSil 972TC-LO

Master Bond

Website:www.masterbond.com
Email:[email protected]
Phone:+1 201 343 8983
Facebook   Twitter   Google Plus   Linkedin
Copyright © 2015 by Master Bond Inc. All Rights Reserved. This content may not be reproduced in any way without the prior written permission of Master Bond Inc.