Master Bond Supreme 11HT-3A is a two part, room temperature curing epoxy system boasting superior toughness. It has a range of high performance properties such as reliable thermal cycling abilities and high temperature resistance. Click below to learn more!

Read More
Some additional key properties include:

Wide service temperature range

-100°F to +400°F [-73°C to +204°C]

High strength profile

Lap shear strength: 2,200-2,400 psi

Coefficient of thermal expansion

45-50 x 10-6 in/in/°C

Hardness at room temperature

75-85 Shore D