EP15
One part epoxy for testing adhesion or cohesive strength of ceramic based flame-sprayed coatings
Key Features
- Used in ASTM C633 testing applications
- Exceptionally high tensile strength
- Excellent dimensional stability
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
40,000-65,000 cps
Cure Schedule
300-350°F for 60-90 minutes, with an optimum cure schedule of 60-90 minutes at 300-350°F plus post cure 4-6 hours at 300-350°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +250°F
Tensile Strength
12,000-14,000 psi
Tensile Lap Shear Strength
2,600-2,800 psi
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
1,000 Hours at 85°C/85% RH
Case Study
EP15: Utilized to test the bond strength of thermal spray according to ASTM C633
Master Bond EP15 is a one-component, thermally-curing epoxy with a tensile strength in excess of 12,000 psi (82.7 MPa) due to the formation of rigid, dimensionally stable bonds upon curing. This bulk tensile strength makes it ideal for testing the ad …
Case Study
Tensile Strength Testing of Aluminum Alloy Coatings According to ASTM Standard C 633-01
Researchers evaluated EP15 when testing SiC-reinforced Al-12Si alloy coatings that were produced using the Cold Gas Dynamic Spraying deposition process. The composite coatings’ bond strengths and microstructures were evaluated, as well as the porosit …