EP35SP Type V

Two component epoxy system for bonding, sealing and coating applications
Key Features
  • Very high temperature resistance
  • Robust resistance to aggressive chemicals
  • Very long open time
  • Good flow properties
Typical Properties
Viscosity
7,000-20,000 cps
Cure Schedule
gel for 1 hour at 110°C followed by 2-3 hours at 125-150°C
Hardness
>75 Shore D
Service Temperature Range
-80°F to +500°F
Dielectric Constant
4.1
Glass Transition Temperature (Tg)
200-210°C
Volume Resistivity
>10¹⁴ ohm-cm
Imagen
EP35SP Type V Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP35SP Type V is a two component epoxy system specially formulated to resist higher temperatures and aggressive chemicals. This lower viscosity material has an easy to use 100 to 50 mix ratio by weight. It will not cure at room temperature and it has an exceptionally long working life, far exceeding 24 hours. Although, it is slightly exothermic, it can be cured in sections exceeding 1/4 inch thick. Particular attention should be paid to the curing schedule. The main attribute of EP35SP Type V is as a high temperature resistant structural type adhesive, although it has many other outstanding properties as well. In this context, it can be used for filament winding, tooling compounds along with bonding composites and pultruded structures. As mentioned previously, it bonds well to a wide variety of substrates, including metals, composites, glass and many plastics. EP35SP Type V is highly resistant to water, oils, acids, bases and solvents. It has top notch physical strength properties and is a superior electrical insulator. The color of Part A is gray, and Part B is amber. The service temperature range for this system is -80°F to +500°F. EP35SP Type V is specified in many applications in aerospace, electronics, optical and specialty OEM, where the special combination of properties described above is needed.

Product Advantages

  • Lower viscosity; very long open time
  • Superb adhesion to a wide variety of substrates
  • Ample physical strength properties
  • Terrific resistance to aggressive chemicals especially acids, bases and petroleum related
  • Commanding high temperature serviceability
  • Excellent compatibility with filament winding and bonding composites
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.