EP41S
Versatile, two part epoxy system for bonding, sealing, coating and encapsulating
Key Features
- Rapid curing; fast handling time
- Exceptional chemical resistance profile
- Impressive physical strength properties
- Widely used for coating tanks and vessels
- Outstanding electrical insulation properties
- Convenient processing
Typical Properties
Viscosity
Part A: 10,000-15,000 cps, Part B: 3,000 - 5,000 cps
Cure Schedule
75°F is 24 hours, 200°F is 60-90 minutes. Optimum cure schedule is overnight at 75°F plus 1-2 hours at 150-200°F.
Hardness
>75 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Constant
3.6
Tensile Modulus
300,000-350,000 psi
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
Packaging