EP45AOHT
Two component epoxy system for bonding and sealing
Key Features
- High temperature serviceability to +500°F
- Very good thermal conductivity
- Exceptionally long working life
- Easily applied
Typical Properties
Viscosity
paste
Cure Schedule
2-3 hours at 300°F followed by a post cure of 3-4 hours at 350°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +500°F
Dielectric Constant
4.6
Tensile Lap Shear Strength
2,300-2,500 psi
Thermal Conductivity
9-10 BTU•in/(ft²•hr•°F) [1.30-1.44 W/(m•K)]
Volume Resistivity
>10¹⁵ ohm-cm