EP50-1.5
Two component, ultra fast setting epoxy system for bonding and sealing
Key Features
- Cryogenic serviceability
- High tensile shear strength
- One to one mix ratio, weight or volume
- Typical fixture time 5-8 minutes at 75°F
- Available in different viscosities or colors
- For repair and high speed production
Typical Properties
Viscosity
Part A: 10,000-16,000 cps, Part B: 50,000-75,000 cps
Cure Schedule
75°F 6-12 hours
Hardness
>70 Shore D
Service Temperature Range
4K to +250°F
Tensile Modulus
>350,000 psi
Volume Resistivity
10¹⁴ ohm-cm