EP21TDCHT

Versatile, toughened two component epoxy for bonding, sealing and coating
Key Features
  • Superb strength profile
  • Dependable electrical insulator
  • Convenient one to one mix ratio
  • Withstands aggressive thermal cycling
  • Ideal for bonding similar and dissimilar substrates
  • Meets MIL-STD-883J Section 3.5.2 for thermal stability
Typical Properties
Viscosity
Part A: 60,000-110,000 CPS, Part B: 70,000-140,000 CPS
Cure Schedule
overnight at 75°F, followed by 1-2 hours at 150-200°F
Hardness
>60 Shore D
Service Temperature Range
-112°F to +350°F
Tensile Lap Shear Strength
>2,700 psi
Tensile Modulus
200,000-250,000 psi
Image
EP21TDCHT Epoxy System
Certifications

Meets EU Directive 2015/863

MIL-STD-883J for Thermal Stability

Product Description

Master Bond EP21TDCHT is a two component epoxy adhesive, sealant and coating featuring high performance, versatility and user friendliness. It has a forgiving and convenient one to one mix ratio by weight or volume. It cures at ambient temperatures and can be accelerated by adding heat, with the optimum cure schedule being overnight at room temperature, followed by 1-2 hours at 150-200°F. This moderate viscosity system bonds well and with minimum shrinkage to a wide variety of substrates including metals, composites, glass, ceramics and many plastics and rubbers. EP21TDCHT combines good dimensional stability with toughness. The forgiving nature of EP21TDCHT allows it to be used for bonding dissimilar substrates that might have different coefficients of thermal expansion, conferring upon it top notch resistance to rigorous thermal cycling as well as vibration and shock. It is a superior electrical insulator and has good chemical resistance against water, fuels and oils. Its service temperature range is from -112°F to +350°F. Part A is clear and Part B is amber in color. It can be used in aerospace, electrical, electronic, medical, specialty OEM and a wide variety of other industries as well.

Product Advantages

  • Convenient mixing: non-critical equal weight or volume ratio
  • User friendly, easy to apply, good flow along with convenient curing schedules
  • Impressive adhesion to a wide variety of substrates
  • Superior toughness, can withstand harsh thermal cycling while retaining dimensional stability
  • Dependable electrical insulation values
  • Robust temperature resistance profile from -112°F to +350°F
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.