UV24TKLO
One component, moderate viscosity, UV curable system meets NASA low outgassing
Key Features
- Excellent physical strength properties
- High dimensional stability
- Superior temperature and chemical resistance
- Not oxygen inhibited
Typical Properties
Viscosity
40,000-55,000 cps
Cure Schedule
UV light 320-365 nm for 20-30 seconds
Hardness
80-85 Shore D
Service Temperature Range
-60°F to +400°F
Dielectric Constant
3.7
Glass Transition Temperature (Tg)
120-130°C
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863