EP34AN-1

Two component, room temperature curing epoxy for bonding, sealing and coating
Key Features
  • Superlative thermal conductivity
  • Exceptional electrical insulation properties
  • Temperature resistance up to +450°F
  • Outstanding thermal cycling capabilities
Typical Properties
Viscosity
paste
Cure Schedule
75°F: 48-72 hours; 200°F: 2-3 hours
Hardness
>85 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.5
Thermal Conductivity
9-10 BTU•in/(ft²•hr•°F) [1.30-1.44 W/(m•K)]
Volume Resistivity
>10¹⁴ ohm-cm
Imagen
EP34AN-1 Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP34AN-1 is a two part, room temperature curing epoxy system for bonding, sealing and coating featuring high temperature resistance, sterling thermal cycling capabilities, first rate thermal conductivity and peerless electrical insulation properties. It is very easy to work with as it has a 100 to 70 mix ratio by weight which works out to a very convenient one to one ratio by volume. This system cures readily at room temperature or more rapidly at elevated temperatures. To optimize its properties, the recommended cure schedule is overnight at room temperature followed by a post cure at 150-200°F for 2-3 hours. Upon polymerization EP34AN-1 is serviceable from -60°F to +450°F. Another noteworthy characteristic is its superior dimensional stability. It resists a range of chemicals including water, oils, fuels and many acids and bases. This thixotropic system bonds well to a wide variety of substrates including metal, composites, glass, ceramics and many rubbers and plastics. As previously mentioned, EP34AN-1 combines thermal conductivity, electrical insulation, the ability to withstand rigorous thermal cycling and an array of superior physical strength properties. EP34AN-1 is 100% reactive and does not contain any diluents or solvents. The color of Part A is gray, Part B is gray. It is widely used in aerospace, electronic, electrical and specialty OEM type applications among others where the combination of properties mentioned above is desirable.

Product Advantages

  • Convenient mixing: one to one ratio by volume
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly
  • High temperature resistance up to 450°F
  • Combines exceptionally high thermal conductivity and fine electrical insulation properties
  • Very good dimensional stability
  • Capable of withstanding rigorous thermal cycling
  • Superb adhesion to a wide variety of substrates

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.