MasterSil 151AN
Two component silicone compound for casting, potting, encapsulation and sealing
Key Features
- Excellent electrical insulation
- High degree of thermal conductivity
- Very good flow properties
- Superb thermal shock resistance
- Low exotherm system
- Suitable for potting, encapsulation and casting
Typical Properties
Viscosity
Part A: 35,000-65,000 cps, Part B: 30-100 cps
Cure Schedule
48-72 hours at 75°F; 2-3 hours at 200°F
Hardness
75-85 Shore A
Service Temperature Range
-65°F to +400°F
Dielectric Strength
450 volts/mil
Elongation
120-150%