EP29LPTCHT
Two component, thermally conductive, electrically insulative epoxy system
Key Features
- Low exotherm, long working life
- Applicable in very thin bond lines
- Excellent flow properties
- Superior dimensional stability
Typical Properties
Viscosity
5,000-15,000 cps
Cure Schedule
overnight at 75°F followed by 4-5 hours at 160°-180°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +350°F
Coefficient of Thermal Expansion
22-24 x 10⁻⁶ in/in/°C
Dielectric Constant
4.4
Imagen
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863
Packaging