Supreme 11HTND
Toughened, two component epoxy for bonding, sealing and coating with paste consistency
Key Features
- Convenient handling
- Excellent toughness
- Withstands thermal cycling
- High bond strength in shear and peel modes
Typical Properties
Viscosity
Part A: paste, Part B: paste
Cure Schedule
overnight at 75°F, followed by 1 hour at 150-200°F
Hardness
75-85 Shore D
Service Temperature Range
-112°F to +400°F
Tensile Lap Shear Strength
3200-3400 psi
Tensile Modulus
300000-350000 psi