Ultra-Low Viscosity, Biocompatible Epoxy Offers Optical Clarity
Master Bond EP4CL-80Med is a one part, optically clear epoxy developed for use in medical device assembly applications. It withstands repeated sterilization cycles and passes ISO 10993-5 testing for non-cytotoxicity. This product cures at moderate temperatures of around 80-85°C within 60 to 90 minutes and faster at slightly higher temperatures. As a one part, non-premixed and frozen system, it contains no solvents, and has an “unlimited” working life at room temperature. Suitable for bonding, sealing, impregnating, and coating, it provides a high glass transition temperature of 155-160°C and has an extremely low viscosity of 50-150 cps at 25°C. This allows it to be applied by brushing, spraying, and spin coating.
EP4CL-80Med provides notable strength properties including a compressive strength of 12,000-14,000 psi and a high tensile modulus of 450,000-500,000 psi at room temperature. It is serviceable over the temperature range of -62°C to +232°C. This compound is an excellent electrical insulator with a volume resistivity of more than 1014 ohm-cm at room temperature and has a refractive index of 1.52 at 25°C. EP4CL-80Med has good resistance to many sterilization methods, including autoclaving, dry heat, radiation, and chemical sterilants. Furthermore, it resists vaporized hydrogen peroxide, a sterilization technology from STERIS®. It bonds well to a variety of substrates such as metals, composites, ceramics, and many plastics. Packaging is available in jars and cans, as well as syringes.
For Editorial Use
Click below to download this release in the format of your choice.
| Adjunto | Tamaño |
|---|---|
| EP4CL-80Med_nr.doc (30.5 KB) | 30.5 KB |
| Adjunto | Tamaño |
|---|---|
| EP4CL-80Med_nr.txt (6.28 KB) | 6.28 KB |
| Adjunto | Tamaño |
|---|---|
| EP4CL-80Med_nr.html (4.02 KB) | 4.02 KB |
News Release Images
Click an image to download a high resolution version in JPEG format.