Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
Two Component Epoxy EP62-1HTMed
EP62-1HTMed
Two component epoxy with superior temperature and chemical resistance that withstands repeated and aggressive sterilization
Glass Transition Temperature (Tg)
145-155°C
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 55,000-110,000 cps, Part B: 100-1,000 cps 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C] 80-90 Shore D -60°F to +450°F /es/tds/ep62-1htmed
EP62-1HTMed Black
Two component epoxy with superior temperature and chemical resistance that withstands repeated and aggressive sterilization
Glass Transition Temperature (Tg)
145-155°C
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
Part A: 55,000-110,000 cps, Part B: 100-1,000 cps 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C] 80-90 Shore D -60°F to +450°F /es/tds/ep62-1htmed-black
Two Part Epoxy EP62-1HTND
EP62-1HTND

Two component epoxy system featuring superior temperature and unsurpassed chemical resistance, especially to acids

Glass Transition Temperature (Tg)
145-155°C
Tensile Modulus
500,000-550,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
Part A: paste, Part B:100-1,000 cps 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]. To obtain optimum properties, post curing at 212-302°F [100-150°C] for 3-5 hours is recommended 80-90 Shore D -60°F to +450°F /es/tds/ep62-1htnd
EP62-1LO Two Part Epoxy
EP62-1LO
High temperature resistant, NASA low outgassing epoxy compound
Dielectric Constant
4.2
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
4,000-8,000 cps 4-6 hours at 60-70°C, 20-40 minutes at 80-100°C or 10 minutes at 125°C 80-90 Shore D -60°F to +450°F /es/tds/ep62-1lo
EP62-1LPSP
Two component, high performance epoxy system featuring convenient handling along with excellent temperature and chemical resistance
Tensile Lap Shear Strength
1,800-2,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Impregnation
  • Potting
  • Underfill
150-300 cps Typical cure conditions range from 8-10 hours at 60-70°C, 60-90 minutes at 80-100°C or 30-60 minutes at 125°C. Post curing at 100-150°C for 3-4 hours will help optimize properties. 75-85 Shore D 4K to +400°F /es/tds/ep62-1lpsp
EP62-1LPSPMed Two Component Epoxy
EP62-1LPSPMed
Two component, high performance epoxy system featuring biocompatibility for bonding, sealing, coating, encapsulating and impregnation
Glass Transition Temperature (Tg)
80-85°C
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Impregnation
  • Potting
  • Underfill
150-300 cps 8-10 hours at 60-70°C, 60-90 minutes at 80-100°C, or 30-60 minutes at 125°C 75-85 Shore D 4K to +400°F /es/tds/ep62-1lpspmed
Two Part Epoxy EP62-1LPSPMed White
EP62-1LPSPMed White
Two component, high performance epoxy system featuring biocompatibility for bonding, sealing, coating, encapsulating and impregnation
Dielectric Constant
4.6
Glass Transition Temperature (Tg)
80-85°C
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Impregnation
  • Encapsulation
  • Potting
  • Gap Filling
150-300 cps Overnight at 75°F followed by either 8-10 hours at 60-70°C, 60-90 minutes at 80-100°C, or 30-60 minutes at 125°C. Post curing at 110-135°C for 2-4 hours will help optimize properties. 75-85 Shore D 4K to +400°F /es/tds/ep62-1lpspmed-white
EP62-1Med Two Component Epoxy System
EP62-1Med
Two component, biocompatible epoxy compound
Dielectric Constant
4.3
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
4,000-8,000 cps Typical cure schedules range from 4-6 hours at 60-70°C, 20-40 minutes at 80-100°C or 10 minutes at 125°C. 80-90 Shore D -60°F to +450°F /es/tds/ep62-1med
EP63 One Part Adhesive System
EP63

One component, moderate viscosity epoxy for bonding and sealing that cures at 80°C to 90°C

Glass Transition Temperature (Tg)
140-150°C
Tensile Modulus
350,000-500,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
35,000-55,000 cps 3-4 hours at 80-90°C followed by post curing at 125°C for 1-2 hours 85-90 Shore D -80°F to +500°F [-62°C to +260°C] /es/tds/ep63
Two Part Epoxy System EP64
EP64

Two component, vacuum compatible epoxy with convienent handling featuring outstanding temperature and chemical resistance

Glass Transition Temperature (Tg)
210-215°C
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
50,000-90,000 cps 80–90°C for 4–6 hours, followed by a post cure at 120–130°C for 2–4 hours 80-90 Shore D -60°F to +450°F [-51°C to +232°C] /es/tds/ep64

Need Expert Guidance?