Supreme 3HTS-80
One component, toughened, silver conductive epoxy system
Tensile Lap Shear Strength
400-500 psi
Volume Resistivity
<0.05 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste Cures at 175°F to 185°F for 2 to 3 hours 50-60 Shore D -100°F to +350°F /es/tds/supreme-3hts-80
Supreme 42HT-2 Two Part Epoxy
Supreme 42HT-2
Two component epoxy system for bonding, sealing, coating and encapsulation
Dielectric Strength
440 volts/mil
Glass Transition Temperature (Tg)
130-135°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
  • Potting
  • Casting
Part A: 75,000-125,000 cps, Part B: 30-70 cps 48-72 hours at 75°F; 2-3 hours at 200°F; overnight at 75°F followed by 3-5 hours at 160-200°F 70-80 Shore D -80°F to +450°F /es/tds/supreme-42ht-2
Supreme 42HT-2ND Two Part Epoxy
Supreme 42HT-2ND
Two component epoxy system for bonding, sealing and coating
Glass Transition Temperature (Tg)
130-135°C
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste overnight at 75°F followed by 3-5 hours at 160-200°F 75-85 Shore D -80°F to +450°F /es/tds/supreme-42ht-2nd
Supreme 42HT-2ND Black Two Part Epoxy
Supreme 42HT-2ND Black
Two component, non-flow epoxy system for bonding, sealing and coating
Dielectric Constant
4.5
Glass Transition Temperature (Tg)
130-135 °C
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 48-72 hours at ambient temperatures and in 2-3 hours at 200°F; optimum cure schedule is overnight at 75°F followed by 3-5 hours at 160-200°F 75-85 Shore D 4K to +450°F /es/tds/supreme-42ht-2nd-black
Supreme 42HT-2ND-2 Two Component Epoxy
Supreme 42HT-2ND-2
Two component epoxy system for bonding, sealing and coating
Glass Transition Temperature (Tg)
130-135°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 48-72 hours at ambient temperatures and in 2-3 hours at 200°F 70-80 Shore D -80°F to +450°F /es/tds/supreme-42ht-2nd-2
Supreme 45HT Two Component Epoxy System
Supreme 45HT
Toughened, two component epoxy system for bonding, sealing and coating
Dielectric Constant
4.5
Tensile Lap Shear Strength
>2,500 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
35,000-60,000 cps 250-300°F for 3-4 hours followed by a post cure at 350-400°F for 1-2 hours 80-90 Shore D -100°F to +450°F /es/tds/supreme-45ht
Supreme 45HTND-2LO Black Two Part Epoxy
Supreme 45HTND-2LO Black
Toughened, two component epoxy system featuring high temperature resistance
Dielectric Constant
4.5
Tensile Lap Shear Strength
2,200-2,400 psi
  • RoHS Compliant
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 250-300°F for 3-4 hours followed by a post cure at 350-400°F for 1-2 hours 80-90 Shore D -100°F to +450°F /es/tds/supreme-45htnd-2lo-black
Supreme 45HTQ Two Part Epoxy Compound
Supreme 45HTQ
Two component epoxy system for bonding, sealing and casting
Tensile Lap Shear Strength
2,100-2,300 psi
Tensile Modulus
500,000-550,000 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Casting
  • Coating
  • Encapsulation
  • Potting
20,000-30,000 cps 4 to 6 hours at 250°F, 4 to 5 hours at 350°F, optimal cure schedule is 300°F for 2 hours, followed by post curing at 350°F for 4 to 6 hours. 80-90 Shore D -60°F to +450°F /es/tds/supreme-45htq
Supreme 45HTQ Two Component Epoxy
Supreme 45HTQ-4
Two component epoxy system for bonding, sealing and casting
Coefficient of Thermal Expansion
30-35 x 10⁻⁶ in/in/°C
Dielectric Constant
4.5
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste At 250°F, the cure time is 4-6 hours but at 300°F, this system will cure in 4-5 hours. 85-90 Shore D -100°F to +450°F /es/tds/supreme-45htq-4
Two Part Epoxy System Supreme46HT-1AO
Supreme 46HT-1AO
Two part, thermally conductive, electrically insulative epoxy for bonding and sealing featuring outstanding heat resistance; requires oven curing
Dielectric Strength
450 volts/mil
Tensile Modulus
600,000-650,000 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
75,000-150,000 cps 2 hours at 300°F, followed by 3-4 hours at 350-400°F. 85-95 Shore D -100°F to +550°F /es/tds/supreme-46ht-1ao

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).