Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
UV26DC
One component ester acrylate system cures with UV plus heat and provides high glass transition temperature
Glass Transition Temperature (Tg)
160-170°C
Refractive Index
1.52
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
500-3,500 cps UV light at 320-365 nm with 20-40 milliwatts/cm2 of energy; heat curing at 125°C for 2-3 hours in shadowed areas 80-90 Shore D -100°F to +400°F /es/tds/uv26dc
UV26DCMed UV Adhesive
UV26DCMed
One component, dual cure system with UV and heat curing mechanisms for bonding and sealing, passes ISO 10993-5 for cytotoxicity
Dielectric Constant
3.85
Glass Transition Temperature (Tg)
160-170°C
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
Part A: 500-3,500 cps, Part B: Cures at 110-125°C for 60-90 minutes, followed by a post cure at 120-150°C for 1-2 hours 80-90 Shore D -60°F to +500°F /es/tds/uv26dcmed
Master Bond UV26SP Epoxy System
UV26SP
One part, low viscosity UV curable system featuring high temperature resistance for bonding, sealing and coating
Glass Transition Temperature (Tg)
160 to 170°C
Refractive Index
1.55
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
250-1,500 cps UV light 320-365 nm for 10-20 seconds 80-90 Shore D -60°F to +500°F /es/tds/uv26sp
X18 One Component Elastomeric System
X18
One component primer/adhesive for polyolefins
Glass Transition Temperature (Tg)
25-30°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Priming
<2,500 cps 75°F for 12-24 hours; 150°F for 1-2 hours -60°F to +200°F /tds/x18
X18Med One Component Primer/Adhesive
X18Med
One component primer/adhesive for polyolefins, passes ISO 10993-5 test
Glass Transition Temperature (Tg)
25-30°C
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Priming
<2,500 cps 30-45 minutes with full cures in 12-24 hours; if cured at 150°F the curing time will be 1-2 hours -60°F to +200°F /es/tds/x18med
X21 Elastomer Based One Component Adhesive
X21
One component primer/adhesive for polyolefins
Glass Transition Temperature (Tg)
25-30°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Priming
<250 cps 12-24 hours at 75°F; 1-2 hours at 150°F -60°F to +200°F /tds/x21
X21Med One Component Elastomeric System
X21Med
One component primer/adhesive for polyolefins, passes ISO 10993-5 test
Glass Transition Temperature (Tg)
25-30°C
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Priming
30-250 cps 12-24 hours at 75°F, 1-2 hours at 150°F -60°F to +200°F /es/tds/x21med