EP125

Two part epoxy for bonding and sealing featuring very high temperature resistance
Key Features
  • High glass transition temperature
  • Meets NASA low outgassing specifications
  • First rate dimensional stability
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
250,000-500,000 cps
Cure Schedule
3-4 hours at 300°F or 2-3 hours at 350°F
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +600°F
Dielectric Constant
3.9
Tensile Lap Shear Strength
2,500-2,700 psi
Image
Epoxy System EP125
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond EP125 is a special two part epoxy that excels in high temperature applications up to +600°F. Its glass transition temperature is exceptionally impressive; 190-200°C. EP125 has slightly different handling properties when compared to other epoxies, but ultimately, is easily processable. Part A is a moderate viscosity liquid and Part B is a powder. When using this system, Part A is heated to 150-160°F, and then appropriate amount of Part B (based on a 100 to 50 mix ratio by weight) is added and stirred into the heated Part A. The mixed system is a malleable paste, with an exceedingly long open time, that is easy applicable. The curing schedule is 3-4 hours at 300°F or 2-3 hours at 350°F. For optimum properties, post curing for 12-24 hours at 400-450°F is strongly recommended.

EP125 bonds well to a wide variety of substrates, including metals, composites, glass, ceramics, rubbers and many plastics. Additionally, it is formulated as a toughened system allowing it to withstand rigorous thermal cycling. EP125 is an elite electrical insulator, especially as it retains compelling insulative properties at very high temperatures. Furthermore, it has superb chemical resistance to water, oils, acids, bases and many solvents. There are a few other notable properties, including remarkably high compressive strength, wonderful dimensional stability and low shrinkage upon curing. EP125 is an excellent candidate for challenging aerospace, electronic, optical, specialty OEM and related applications where these formidable attributes are desirable.

Product Advantages

  • Excellent long-term thermal stability
  • Superior electrical insulation properties
  • 100% reactive—no solvents or other volatiles
  • High adhesion to metallic and non-metallic substrates
  • Robust physical strength profile especially in the compressive mode
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.