Two component, silver filled epoxy adhesive, sealant
Key Features
- One to one mix ratio
- Paste consistency
- Cures at ambient temperature
- Excellent electrical conductivity
Typical Properties
Viscosity
Paste
Cure Schedule
2-3 days at 75°F, 2-3 hours at 125-150°F, 1-2 hours at 200°F
Hardness
45-55 Shore D
Service Temperature Range
-60°F to +300°F