UV15DC80
One component, UV and heat curable epoxy compound with moderate viscosity
Key Features
- Allows for curing in “shadowed out” areas
- Cures at temperatures as low as 80°C
- Convenient no mix system
- Excellent physical strength properties
Typical Properties
Viscosity
45,000-60,000 cps
Cure Schedule
10-20 seconds with UV light at 365 nm with 20-40 milliwatts/cm2 of energy; areas not cured by shadowing can be cured at 80°C for 2-3 hours; post curing for 2-4 hours will help optimize properties; if possible, 1-2 hours at 125°C will promote curing even further
Hardness
>70 Shore D
Service Temperature Range
-80°F to +350°F
Glass Transition Temperature (Tg)
125-135°C
Volume Resistivity
>10¹⁴ ohm-cm
Immagine
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
Case Study
UV15DC80: Utilized in ultraviolet-assisted three-dimensional printing
Researchers at Ecole Polytechnique de Montreal manufactured photopolymer-based microdevices with 3D self-supported and freeform structures. The investigated photopolymers included a polyurethane-based resin and Master Bond UV15DC80.