UV15X-6Med-2
UV system for high performance bonding, sealing and coating
Key Features
- Superior abrasion resistance
- Passes USP Class VI testing
- High flexibility and toughness
- Moderate viscosity
Typical Properties
Viscosity
35,000-55,000 cps
Cure Schedule
Cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2.
Hardness
25-45 Shore D
Service Temperature Range
-80°F to +250°F
Elongation
>100%
Refractive Index
1.50
Immagine
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
USP Class VI Medical
Meets EU Directive 2015/863
ISO 10993-5 for Cytotoxicity
Case Study
UV15X-6Med-2: Used as a Biocompatible Encapsulant for a Wireless, Nerve Stimulation System
In this case study, UV15X-6Med-2, a one part UV curable medical grade adhesive, provided a biocompatible barrier for a closed-loop, wireless implantable device.