MasterSil 151AO
Two part silicone for high performance casting, potting & encapsulation and sealing
Key Features
- Superior thermal conductivity
- Low exotherm; very long pot life
- Excellent flexibility
- Superb electrical insulation properties
- Can cure in thicknesses up to and beyond 1-2 inches
- High temperatures resistance to +400°F
Typical Properties
Viscosity
Part A: 17,000-24,000 cps, Part B: 50-150 cps
Cure Schedule
48-72 hours at 75°F, 2-3 hours at 200°F
Hardness
75-85 Shore A
Service Temperature Range
-65°F to +400°F
Coefficient of Thermal Expansion
120-150 X 10⁻⁶ in/in/°C
Dielectric Strength
450 volts/mil
Immagine
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
MIL-STD-810G for Fungus Resistance
Meets EU Directive 2015/863