LED405FL3

One component, flexibilized LED curable system
Key Features
  • Fast cure with appropriate LED light
  • Not oxygen inhibited
  • Outstanding optical clarity, with fluorescent dye
  • Can cure up to 1/8 inch thick
Typical Properties
Viscosity
500-3,000 cps
Cure Schedule
Cure with LED at 405 nm at ~ 1-4 watts/cm² intensity for 15-30 seconds or longer in thicker sections.
Hardness
5-15 Shore D
Service Temperature Range
-100°F to 250°F
Refractive Index
1.51
Volume Resistivity
>10¹⁴ ohm-cm
Immagine
LED405FL One Part LED Curable Adhesive
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond LED405FL3 is a one part system that cures upon exposure to LED light at 405 nm. It will cure rapidly and fully without any oxygen inhibition. Significantly, a UV light source is not needed to achieve polymerization. The speed of cure depends upon the intensity of the light source, the thickness of the layer, and the distance of the light source from the material being cured. The intensity of the light should be 2-4 watts/cm2. Thinner sections will typically cure in 30-45 seconds. Thicker sections will take longer.

LED405FL3 bonds well to a wide variety of substrates including plastics, glass and metals. A salient feature is its flexibility, which allows the system to be compatible for bonding materials with different coefficients of thermal expansion. Additionally, it can withstand rigorous thermal cycling, mechanical shock and vibration. It is a reliable electrical insulator with a service temperature range of -100°F to 250°F. LED405FL3 resists many chemicals including mild acids, bases, oils, fuels and water. In fact, a cured sample withstood 12 hours of immersion in hot water (90°C) without any significant change in weight. The system is a good candidate for applications in aerospace, opto-electrical, optical, and specialty OEM, where a strong, flexible LED curable system is desirable.

Product Advantages

  • One component system, needs no mixing
  • Cures by LED light, UV light not required
  • Superb flexibility, withstands thermal cycling
  • Can be used for small pottings and encapsulation
  • Especially resistant to water
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.