EP21LV-LO
Two component, low viscosity NASA low outgassing epoxy compound
Key Features
- One to one mix ratio by weight
- High bond strength
- Superior electrical insulation properties
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
10,000-13,000 cps
Cure Schedule
overnight at 75°F followed by 2 hours at 150-200°F
Hardness
70-80 Shore D
Service Temperature Range
-65°F to +250°F
Dielectric Constant
2.79
Tensile Lap Shear Strength
2,600-2,800 psi