Supreme 46HTQ
Two component epoxy system for bonding, sealing and casting
Key Features
- High temperature resistant
- Outstanding compressive strength
- Superior abrasion resistance
- Exceptional chemical resistance
Typical Properties
Viscosity
10,000-25,000 cps
Cure Schedule
4-6 hours at 250°F and 3-4 hours at 300°F
Hardness
85-95 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.6
Tensile Lap Shear Strength
2,000-2,200 psi