UV15DC80-10

One component, UV and heat curable epoxy compound with low to moderate viscosity
Key Features
  • Allows for curing in “shadowed out” areas
  • Cures at temperatures as low as 80°C
  • Convenient no mix system
  • Excellent physical strength properties
Typical Properties
Viscosity
8,000-12,000 cps
Cure Schedule
Cures at temperatures as low as 80°C. Areas not cured because of shadowing can be cured at 80°C for 40-60 minutes. Post curing at 125-150°C for 15-30 minutes can increase the T from 90°C achieved by straight UV curing to over 125°C.
Hardness
>70 Shore D
Service Temperature Range
-80°F to +350°F
Glass Transition Temperature (Tg)
>125°C
Volume Resistivity
>10¹⁴ ohm-cm
Immagine
One Part UV and Heat Curable Compound
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond UV15DC80-10 is a special dual cure epoxy based system which offers a primary cure utilizing UV light along with a secondary heat curing mechanism. This system addresses the problem of curing areas on parts that do not allow UV light curing because of “shadowing” issues. Most noteworthy is that the heat cure portion can be initiated at only 80°C rather than at the more common 125°C. Another very useful feature of a dual cure UV is that it allows for rapid fixturing and then enables the cure to be completed by adding heat. As alluded to above, a secondary cure at 80°C is not very common and highly desirable because of the sensitivity of many plastics to elevated temperatures. Also, the decrease of fixturing time to seconds is highly advantageous in a production environment, or when fixturing is a laborious and expensive proposition. One innovative use of a dual cure UV is to fixture two optically opaque substrates, such as metals, with the UV light exposure and then completing the cure with heat.

This high viscosity system features a cationic cure mechanism (for the UV portion) and has exceptionally low shrinkage upon curing. UV15DC80-10 is not oxygen inhibited and has outstanding chemical resistance to many acids, bases, fuels and solvents. It is a superb electrical insulator and bonds well to metals, glass, ceramics and most plastics. UV15DC80-10 has a service temperature range of -80°F to +350°F.

Straight UV curing can be accomplished for thicknesses of 0.010” to 0.020” in seconds using UV light at 365 nm with 20-40 milliwatts/cm2 of energy. Faster cures can be achieved at higher energy outputs. Areas not cured because of shadowing can be cured at 80°C for 40-60 minutes. In addition, post curing at 125-150°C for 15-30 minutes can increase the Tg from 90°C achieved by straight UV curing to over 125°C. The 80°C secondary cure is truly a remarkable innovation. It has wide applicability in the optical, electronic and optoelectronic industries.

Product Advantages

  • One component system; no mixing needed
  • Dual cure capability; UV, heat, or both
  • No oxygen inhibition
  • Bonds well to a wide variety of substrates
  • Excellent physical strength properties
  • Low to moderate viscosity, no solvents or diluents
    Show More

    How to order

    Verify Your Product Selection

    With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

    Get a Quote

    Our customer service team will follow up with a detailed quote with packaging and shipping options.

    Place Your Order

    We'll work with your company to process the order efficiently.

    Receive Your Material

    Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.