Supreme 45HT-3

Two component, quartz filled epoxy system for bonding, sealing and casting
Key Features
  • Very long open time
  • High temperature resistance
  • Exceptional compressive strength
  • Withstands abrasive forces
Typical Properties
Viscosity
50,000-100,000 cps
Cure Schedule
250°F for 6 to 8 hours, or 4 to 6 hours at 350°F; optimal cure schedule is 300°F for 2 to 3 hours, followed by a post cure at 350°F for 4 to 6 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +550°F
Dielectric Constant
4.5
Glass Transition Temperature (Tg)
145-155°C
Tensile Modulus
550,000-600,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
Immagine
Master Bond Supreme 45HT-3 Epoxy System
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond Supreme 45HT-3 is a two component, toughened epoxy system for high performance bonding, sealing and casting. It has a forgiving 100 to 15 mix ratio by weight. The working life after mixing is 12-24 hours and it provides moderate to high viscosity with good flow. The system requires oven curing at 250°F for 6 to 8 hours, or 4 to 6 hours at 350°F. The optimal cure schedule is 300°F for 2 to 3 hours, followed by a post cure at 350°F for 4 to 6 hours. It is 100% reactive without any solvents or diluents. Supreme 45HT-3 has very low linear as well as volumetric shrinkage upon curing.

Supreme 45HT-3 bonds well to a wide variety of substrates, including metals, composites, ceramics and many different plastics. After curing, it has a number of desirable physical strength properties including a high modulus and exceptional compressive strength. It is a toughened system that can withstand rigorous thermal cycling. This epoxy excels in withstanding chemicals seen in downhole environments, be it acids, bases or solvents. The presence of the quartz filler confers enhanced dimensional stability and increased abrasion resistance. Supreme 45HT-3 is a reliable electrical insulator. It is a relatively high Tg epoxy with a service temperature range from -100°F to +550°F. The color of Part A is tan and Part B is brown. Everything considered, Supreme 45HT-3 is a versatile system that can be used in aerospace, electronic, oil and chemical processing, specialty OEM, and similar type applications.

Product Advantages

  • Long working life
  • Low linear and volumetric shrinkage upon curing
  • Extremely chemical resistant
  • High glass transition temperature
  • Impressive compressive strength
  • Robust dimensional stability
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.