MasterSil 323Med
Two component, medical grade silicone for bonding and sealing
Key Features
- Addition cured
- Convenient processing
- Excellent strength properties
- Meets ISO 10993-5
Typical Properties
Viscosity
Part A: 15,000-30,000 cps, Part B: 10,000-25,000 cps
Cure Schedule
75°F: 48-72 hours; 135-165°F: 2-4 hours; Optimal cure: Overnight at 75°F followed by 2-4 hours at 135-165°F
Hardness
35-45 Shore A
Service Temperature Range
-65°F to +400°F
Acoustical Impedance
1.1 MRayl
Elongation
150-250%