EP62-1HTMed Black

Two component epoxy with superior temperature and chemical resistance that withstands repeated and aggressive sterilization
Key Features
  • Long open time at room temperature
  • Cures at moderately elevated temperatures
  • Superb physical strength profile
  • Passes ISO 10993-5
Typical Properties
Viscosity
Part A: 55,000-110,000 cps, Part B: 100-1,000 cps
Cure Schedule
60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Glass Transition Temperature (Tg)
145-155°C
Volume Resistivity
>10¹⁴ ohm-cm
Immagine
Applications
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Product Description

Master Bond EP62-1HTMed Black is a two component epoxy system with a long working life at ambient temperature. The mix ratio is a forgiving 100 to 5 by weight. Upon mixing, it is a moderate viscosity system that flows well. The working life of 100 grams is 12-24 hours at room temperature. The cure schedule options are as follows, 60-70 minutes at 176-212°F [80-100°C] or 20-30 minutes at 257°F [125°C]. However to obtain optimum properties, post curing at 212-302°F [100-150°C] for 3-5 hours is strongly recommended. The epoxy contains no solvents or diluents and has low shrinkage upon cure.

The system bonds well to a wide variety of substrates such as metals, plastics, rubbers, ceramics and composites. Upon curing with the optimum schedule, EP62-1HTMed Black excels in combining high temperature resistance along with the ability to withstand repeated sterilization and many aggressive chemicals. It has a high glass transition temperature. EP62-1HTMed Black is a dependable electrical insulating material. The service temperature range is -60°F to +450°F. The color of Part A is black and Part B is dark brown. It is especially well suited for applications where harsh sterilants are being employed.

Product Advantages

  • Very long working life
  • Good flow properties
  • Versatile curing schedules
  • Highly resistant to aggressive chemicals
  • Withstands repeated sterilization including autoclaving
  • Good color compatibility with most endoscopes
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.