UV26DCMed

One component, dual cure system with UV and heat curing mechanisms for bonding and sealing, passes ISO 10993-5 for cytotoxicity
Key Features
  • Low viscosity
  • Minimal shrinkage upon curing/li>
  • Superb optical clarity
  • Cures at 110-125°C in shadowed out areas
Typical Properties
Viscosity
Part A: 500-3,500 cps, Part B:
Cure Schedule
Cures at 110-125°C for 60-90 minutes, followed by a post cure at 120-150°C for 1-2 hours
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +500°F
Dielectric Constant
3.85
Glass Transition Temperature (Tg)
160-170°C
Image
UV26DCMed UV Adhesive
Applications
Certifications

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Product Description

Master Bond UV26DCMed is a dual-cure epoxy system designed for medical applications. It utilizes UV light for the initial cure and heat to fully polymerize areas not directly exposed to UV. Upon exposure to UV light at 320–365 nm with an energy intensity of 20–40 milliwatts/cm², cross-linking occurs rapidly in those areas exposed to the light, with faster cures achievable at higher energy outputs. To ensure complete polymerization, heat must be applied at 110–125°C for 60–90 minutes. Post curing at 120–150°C for 1–2 hours is strongly recommended to optimize physical strength, chemical resistance, and glass transition temperature. In fact, longer heating will further improve these properties. This process ensures thorough and reliable curing, even in complex geometries.

UV26DCMed bonds well to a wide variety of substrates including metals, glass, ceramics and most plastics. It is highly resistant to acids, bases, solvents, and numerous sterilants. These include ethylene oxide, glutaraldehyde, and an array of hydrogen peroxide systems including STERRAD™. Additionally it withstands repeated steam autoclaving. UV26DCMed is a lower viscosity system with exceptionally low shrinkage and outstanding dimensional stability. It is not oxygen inhibited. It is a superb electrical insulator, and is able to withstand rigorous thermal cycling. The service temperature range is -60°F to +500°F. UV26DCMed is recommended for medical device manufacturing, particularly for reusable instruments that require repeated sterilization, especially autoclaving and aggressive liquid sterilants.

Product Advantages

  • One component system, no mixing needed
  • Cures in shadowed out areas with heat
  • No oxygen inhibition
  • Excellent physical strength properties
  • Resists repeated sterilization including autoclaving
  • Passes ISO 10993-5
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.