Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
Two Part Epoxy System EP64Med
EP64Med

Two component, medical grade epoxy with convienent handling featuring outstanding temperature and chemical resistance

Glass Transition Temperature (Tg)
210-215°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • ISO 10993-5 for Cytotoxicity
  • Bonding
  • Sealing
  • Coating
50,000-90,000 cps 80-90°C for 4-5 hours, followed by a post cure at 120-130°C for 2-3 hours 80-90 Shore D -60°F to +450°F [-51°C to +232°C] /it/tds/ep64med
EP65 Two Component Epoxy
EP65
Two component epoxy system featuring fast setup time and good temperature resistance
Dielectric Constant
4.1
Tensile Lap Shear Strength
1,100-1,300 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 11,000-15,000 cps, Part B: 8,000-12,000 cps full cure generally occurs within 12-24 hours 75-85 Shore D -60°F to +300°F /it/tds/ep65
EP65HT Two Component Epoxy
EP65HT
Two component epoxy system featuring the special combination of fast setup times and high temperature resistance
Glass Transition Temperature (Tg)
125-130°C
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: 55,000-110,000 cps, Part B: 8,000-12,000 cps 10-15 minutes setup, full cure within 12-18 hours at 75°F 75-85 Shore D -60°F to +400°F /it/tds/ep65ht
EP6STC-80
EP6STC-80

One component, highly thermally conductive, silver filled epoxy, cures at 80-90°C

Thermal Conductivity
13-14 W/(m•K)
Volume Resistivity
<0.001 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
Thixotropic 85-95 Shore D -60°C to +150°C /tds/ep6stc-80
EP70CN
Two component epoxy system for bonding, sealing, coating and potting featuring a natural curing agent
Tensile Strength
11,000-12,000 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
2,500-5,000 cps overnight at 75°F followed by 3-4 hours at 140-170°F 75-85 Shore D -100°F to +450°F /it/tds/ep70cn
EP75-1 Two Part Epoxy System
EP75-1
Two component, graphite conductive epoxy system for bonding, sealing, coating
Coefficient of Thermal Expansion
10-15 X 10⁻⁶ in/in/°C
Volume Resistivity
50-100 ohm-cm
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: paste, Part B: 200-500 cps overnight at 75°F followed by 1-2 hours at 150-200°F 75-85 Shore D 4K to +250°F /it/tds/ep75-1
 EP76M Two Part Epoxy
EP76M
Two component, nickel filled epoxy for bonding, sealing and coating
Tensile Lap Shear Strength
>2,000 psi
Volume Resistivity
5-10 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: >500,000 cps, Part B: >900,000 cps ambient temperatures in 3-5 days or at 200°F in 2-3 hours >80 Shore D -60°F to +250°F /it/tds/ep76m
EP77M-1 Two Part Epoxy
EP77M-1
Two component, silver conductive epoxy adhesive system
Thermal Conductivity
20-22 BTU•in/(ft²•hr•°F)[2.88-3.17 W/(m•K)]
Volume Resistivity
<10⁻³ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Part A: >400,000 cps, Part B: 10-35 cps overnight at 75°F followed by 1-2 hours at 150°F 70-80 Shore D -60°F to +300°F /it/tds/ep77m-1
EP77M-F
Two component, silver conductive epoxy adhesive system
Thermal Conductivity
10-12 BTU•in/(ft²•hr•°F) [1.44-1.73 W/(m•K)]
Volume Resistivity
10⁻³ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 24 hours at 75°F 40-50 Shore D -100°F to +250°F /it/tds/ep77m-f
EP77M-FMed Two Part Epoxy
EP77M-FMed
Two component, silver conductive epoxy adhesive system for medical applications
Thermal Conductivity
10-12 BTU•in/(ft²•hr•°F) [1.44-1.73 W/(m•K)]
Volume Resistivity
10⁻³ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 24 hours at 75°F 40-50 Shore D -100°F to +250°F /it/tds/ep77m-fmed

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).