Product Selector

Filters
Applications
Product Type
Certifications
Thermal Conductivity
Product Certifications Applications Viscosity Cure Schedule Hardness Temp. Range Link to Content
EP19HT One Component Epoxy System
EP19HT
One component epoxy system for impregnation, lamination, sealing and coating
Dielectric Constant
3.6
Glass Transition Temperature (Tg)
120-125°C
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Impregnation
300-700 cps 1 hour at 250°F followed by a post cure of 1-2 hours at 300-350°F. 80-90 Shore D -60°F to +400°F /it/tds/ep19ht
EP19HTFL One Part Epoxy
EP19HTFL
One component epoxy system for impregnation, lamination, sealing and coating
Glass Transition Temperature (Tg)
125-130°C
Tensile Modulus
>300,000 psi
  • RoHS Compliant
  • Sealing
  • Coating
  • Impregnation
300-700 cps 1 hour at 250°F followed by a post cure of 1-2 hours at 300-350°F >65 Shore D -60°F to +350°F /it/tds/ep19htfl
EP19HTLV One Component Epoxy
EP19HTLV
One component epoxy system for impregnation, lamination, sealing and coating
Dielectric Constant
3.6
Volume Resistivity
>10¹⁵ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Impregnation
300-800 cps Optimum curing schedule is 1 hour at 250°F followed by a post cure of 1-2 hours at 300-350°F. >65 Shore D -60°F to +400°F /it/tds/ep19htlv
EP19HTLV-2 One Part Epoxy System
EP19HTLV-2
One component epoxy system for impregnation, lamination, sealing and coating
Dielectric Constant
3.6
Glass Transition Temperature (Tg)
125-130°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Impregnation
200-700 cps Curing schedule options include 250°F for 60-90 minutes or 300°F for 45-60 minutes. >65 Shore D -60°F to +400°F /it/tds/ep19htlv-2
EP21 Two Component Epoxy Compound
EP21
Two component, room temperature curing epoxy compound
Dielectric Constant
2.9
Tensile Lap Shear Strength
2,800-3,000 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
Part A: 28,000-42,000 cps, Part B: 45,000-65,000 cps 75°F: 48-72 hours; 200°F: 2-3 hours; Optimum cure schedule: overnight at 75°F, plus 2-3 hours at 150-200°F 70-80 Shore D -60°F to +250°F /it/tds/ep21
EP21AC Epoxy Potting Compound
EP21AC
Two component epoxy system for encapsulating and coating that passes UL746A high amp arc ignition at 3.0 mm thickness with a PLC of 0
Dielectric Constant
2.89 at 9.375 GHz
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • UL 94HB for Flame Retardancy
  • UL 746A for High Amp Arc Ignition Resistance
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Potting
30,000-50,000 cps 75°F: 48-72 hours; 150-175°F: 2-3 hours; Optimal cure: Overnight at 75°F followed by 4-6 hours at 135-165°F 75-85 Shore D -75°F to +194°F /it/tds/ep21ac
EP21AOLV Two Component Epoxy
EP21AOLV
Two component epoxy compound for bonding, sealing, coating and potting
Dielectric Constant
4.7
Tensile Lap Shear Strength
1,400-1,600 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation
  • Gap Filling
Part A: 40,000-60,000 cps, Part B: 50,000-70,000 cps overnight at 75°F followed by 3-5 hours at 150-200°F 85-95 Shore D -60°F to +250°F /it/tds/ep21aolv
EP21AOLV-1 Two Part Epoxy
EP21AOLV-1
Two component epoxy compound for bonding, sealing, coating and encapsulating
Coefficient of Thermal Expansion
22-25 X 10⁻⁶ in/in/°C
Dielectric Strength
450 volts/mil
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
  • Casting
  • Potting
Part A: 4,000-8,000 cps, Part B: 50,000-65,000 cps overnight at 75°F followed by 3-5 hours at 150-200°F 85-95 Shore D -60°F to +250°F /it/tds/ep21aolv-1
EP21AOLV-2LO Two Component Epoxy
EP21AOLV-2LO
Two component epoxy compound for bonding, sealing, coating and encapsulating
Coefficient of Thermal Expansion
22-25 X 10⁻⁶ in/in/°C
Dielectric Strength
400-450 volts/mil
  • NASA Low Outgassing
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • MIL-STD-810G for Fungus Resistance
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: 1,500-3,000 cps, Part B: 55,000-125,000 cps 75°F: 3-4 days; 200°F: 2-3 hours; Optimum cure schedule: overnight at 75°F followed by 3-4 hours at 150-200°F 75-85 Shore D -60°F to +250°F /it/tds/ep21aolv-2lo
EP21AOLV-2Med Two Part Epoxy Adhesive
EP21AOLV-2Med
Two component epoxy compound for bonding, coating, sealing and encapsulation
Coefficient of Thermal Expansion
22-25 x 10⁻⁶ in/in/°C
Dielectric Strength
>400 volts/mil
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Potting
  • Gap Filling
  • Casting
Part A: 1,500-3,000 cps, Part B: 50,000-150,000 cps overnight at 75°F followed by 2-4 hours at 150-200°F >80 Shore D -60°F to +250°F /it/tds/ep21aolv-2med

Need Expert Guidance?

Our expert engineers offer one-on-one consultations to help you navigate our extensive material library and find the right solution for your application. We ensure confidentiality and quick turnaround (1-2 business days).