B-Staged Solid at Room Temperature
EP36 Series cookies ship as solid preforms in 22 or 30 gram sizes. For maximum shelf life, ideal storage is in a refrigerator at 40–50°F. They have an "unlimited" working life at room temperature and require no mixing.