Master Bond EP30-4Med Adhesive

EP30-4Med
Optically Clear Epoxy

Passes ISO 10993-5 Certification for Cytotoxicity

PERFORMANCE PROPERTIES

Refractive
index, 75°F

viscosity, 75°F

FOR MEDICAL DEVICE MANUFACTURING

VOLUME RESISTIVITY, 75°F


Chemical Resistance

SERVICE TEMPERATURE RANGE

APPLICATION PROCESS

EP30-4Med can be easily applied with a gun dispenser and offers a convenient 2:1 mix ratio. Its low viscosity makes it ideal for small potting and encapsulation applications.

The compound cures quickly, even in thin sections with a set up time of about 30 minutes depending on application specifics. EP30-4Med offers a working life of 10-15 minutes per 100 gram batch.

PRODUCT ADVANTAGES

1

Ideal for small potting and encapsulation applications

2

ISO 10993-5 certified for cytotoxicity

3

Fast set up time, cures at room temperature

4

Easy mixing with a 2:1 mix ratio by weight

5

Specialty packaging available in gun dispenser

6

Resists EtO sterilization as well as most other liquid sterilants